Method Statement For Damaged Cracked Concrete Repair Of Large Cracks
This procedure shall apply to the repair of all defective cracked concrete in large quantities, using high strength, free flowing, cementitious micro concrete of size 40 – 300 mm thickness. Concrete Preparation The areas to be repaired are to be as shown